S355K2G3 DIN EN 10025-2Number: 1.0595 |
Comparison of steel grades |
|
EN10025:1990 |
FE 510 DD1 |
|
DIN17100 |
- |
|
NFA 35-501 |
E36-4 |
|
BS1449 |
50DD |
|
UNI7070 |
- |
S355K2G3 Chemical analysis -% by mass*
Chemical elements |
C≤ 16mm max |
C>16mm max |
Si max |
Mn max |
P max. |
S max. |
%,by mass |
0.20 |
0.20 |
0.55 |
1.60 |
0.035 |
0.035 |
S355K2G3 Mechanical properties
thickness |
Yield StrengthReH[N/mm2] transv.min. |
TensileStrengthRm |
Fracture Elongation[%]transv. min. |
Notch Impact Energy1)Ch Vcomplete samplelongitud. min [J] |
t≤ 16mm t >16mm |
355 345 |
-20 degree 40J |
||
t < 3mm t ≥ 3mm |
510-680 490-630 |
|||
Up to 1.5mm 1.51-2.00mm 2.01-2.50mm 2.51-2.99mm ≥ 3mm |
13 14 15 16 20 |